Stal żaroodporna - Gatunki PN-H-86022:1971
norma zastąpiona przez PN-EN 10095:2002
oznaczenie PN | odpowiednik PN-EN 10088-1 | odpowiednik PN-EN 10095 | inne normy EN |
H5M | - | - | |
H6S2 | 1.4713 - X10CrAlSi7 | 1.4713 - X10CrAlSi7 | - |
2H17 | 1.4016 - X6Cr17 | 1.4742 - X10CrAlSi18 | - |
H13JS | 1.4724 - X10CrAlSi13 | 1.4724 - X10CrAlSi13 | - |
H18JS | 1.4742 - X10CrAlSi18 | 1.4742 - X10CrAlSi18 | - |
H24JS | 1.4762 - X10CrAlSi25 | 1.4762 - X10CrAlSi25 | - |
H25T | - | - | - |
H26N4 | - | - | - |
H18N9S | 1.4828 - X15CrNISi20-12 | 1.4828 - X15CrNISi20-12 | - |
H23N13 | 1.4833 - X12CrNi23-13 | 1.4833 - X12CrNi23-13 | - |
H20N12S2 | 1.4828 - X15CrNISi20-12 | 1.4828 - X15CrNISi20-12 | - |
H23N18 | 1.4845 - X8CrNi25-21 | 1.4845 - X8CrNi25-21 | 1.4591 - X6CrNi25-20 - PN-EN 10302 |
H25N20S2 | 1.4841 - X15CrNiSi25-21 | 1.4841 - X15CrNiSi25-21 | - |
H18N25S2 | - | - | - |
H16N36S2 | 1.4864 - X12NiCrSi35-16 | 1.4864 - X12NiCrSi35-16 | - |
H9S2 | - | - | 1.4718 - X45CrSi9-3 EN 10090 |
H10S2M | - | - | 1.4731 - X40CrSiMo10-2 EN 10090 |
4H14N14W2M | - | - | |
50H21G9N4 | - | - | 1.4871 - X53CrMnNiN21-9 EN 10090 |